Q. At what thickness do you take side bends for Procedure and Qualification Tests?

A. This depends on the standard that you are working to and the parent material thickness.  If you were testing to BS EN ISO 15614-1:2004+A2 and the parent material was greater or equal to 12mm you would take side bends.  If you were testing to ASME IX: 2013 and the parent material was greater or equal to 10mm you would take side bends.